Replying to Wei et al. Nature Communications https://doi.org/10.1038/s41467-019-13492-9 (2019)
The manuscript entitled “Conformational fitting of a flexible oligomeric substrate does not explain the enzymatic PET degradation” by Wei et al.1 raises a question on the conclusion reached in our published work, particularly regarding the docking calculations of PET substrate into the PETase from Ideonella sakaiensis (IsPETase)2. The authors showed the ethylene glycol torsion angle Ψ in an amorphous PET material of 0.25 mm thickness (Goodfellow Cambridge Ltd.) using solid-state nuclear magnetic resonance experiments and determined trans/gauche ratio of 9:91 at 30 °C in good agreement with the previous report on amorphous PET (14 ± 5%)3. Based on the result, they suggested that the conformation of the docked 2-HE(MHET)4 in our published work that showed a trans content of ethylene glycol higher than 25% is rarely present in amorphous PET polymer chains, and claimed that the residues in subsite IIb and IIc we suggested are unlikely to interact with the two MHET moieties of 2-HE(MHET)4. To support the latter statement, they further demonstrated that the transition from gauche to trans conformation is highly restricted in amorphous PET at 30 °C by magic-angle-spinning nuclear magnetic resonance method. They also suggested that, instead of the perfect accommodation, the key factor facilitating the substrate binding seems to be the fragile contact between the phenylene moieties and the surrounding hydrophobic residues. In general, we agree that the comments by Wei et al. provide concrete experimental results showing that ethylene glycol units of amorphous PET polymer do not have the free rotational properties to fit into its substrate binding site as the form of 2-HE(MHET)4 at 30 °C. Thus, the study provides the scientific community with useful information on PET degradation by IsPETase.
However, our previous docking calculations2 were independent of temperature setting and not restricted to the temperature of 30 °C. Although IsPETase cannot maintain its activity at high temperature due to its low thermal stability, efforts to increase thermal stability of the enzyme have already been reported4. Thus, an engineered IsPETase with high thermal stability might be able to accommodate the PET substrate in the manner we presented at temperatures higher than 30 °C as the trans content of the material was increased to 56% at 70 °C1.
Moreover, we did not use the Goodfellow amorphous PET in our published works2,4, which counters the comment that IsPETase showed almost “no” activity against crystalline PET polymer1. It was also previously shown that the semi-crystalline PET material exhibits much higher trans conformation of ethylene glycol than amorphous one at ambient temperature3. Thus, we believe that the authors’ claims regarding the residues in subsite IIb and IIc may not apply under all conditions. In sum, while we agree that Wei et al. provide useful evidences that the used docking calculation is not suitable in amorphous PET at low temperature such as 30 °C, their observations are not necessarily incompatible with the general findings of our previous work2. We anticipate that Wei et al.’s work and our own will inspire future studies aimed at unraveling the exact mechanisms of PET degradation.
Data availability
Data supporting the findings of this study are available within the article and from the corresponding author upon reasonable request.
References
Wei, R. et al. Conformational fitting of a flexible oligomeric substrate does not explain the enzymatic PET degradation. Nat. Commun. (2019).
Joo, S. et al. Structural insight into molecular mechanism of poly(ethylene terephthalate) degradation. Nat. Commun. 9, 382 (2018).
Schmidt-Rohr, K., Hu, W. & Zumbulyadis, N. Elucidation of the chain conformation in a glassy polyester, PET, by two-dimensional NMR. Science 280, 714–717 (1998).
Son, H. F. et al. Rational protein engineering of thermo-stable PETase from Ideonella sakaiensis for highly efficient PET degradation. ACS Catal. 9, 3519–3526 (2019).
Acknowledgements
This work was supported by the Technology Development Program to Solve Climate Changes on Systems Metabolic Engineering for Biorefineries from the Ministry of Science and ICT (MSIT) through the National Research Foundation (NRF) of Korea (NRF-2012M1A2A2026556 and NRF2012M1A2A2026557).
Author information
Authors and Affiliations
Contributions
H.S., S.Y.C., S.Y.L., and K.-J.K. wrote the initial paper. H.S., I.J.C., S.J., H.F.S., H.-Y.S., S.Y.C., S.Y.L., and K.-J.K. finalized the paper.
Corresponding authors
Ethics declarations
Competing interests
The authors declare no competing interests.
Additional information
Publisher’s note Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.
Rights and permissions
Open Access This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons license, and indicate if changes were made. The images or other third party material in this article are included in the article’s Creative Commons license, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons license and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this license, visit http://creativecommons.org/licenses/by/4.0/.
About this article
Cite this article
Seo, H., Cho, I.J., Joo, S. et al. Reply to “Conformational fitting of a flexible oligomeric substrate does not explain the enzymatic PET degradation”. Nat Commun 10, 5582 (2019). https://doi.org/10.1038/s41467-019-13493-8
Received:
Accepted:
Published:
DOI: https://doi.org/10.1038/s41467-019-13493-8
This article is cited by
-
Emerging Roles of PETase and MHETase in the Biodegradation of Plastic Wastes
Applied Biochemistry and Biotechnology (2021)
Comments
By submitting a comment you agree to abide by our Terms and Community Guidelines. If you find something abusive or that does not comply with our terms or guidelines please flag it as inappropriate.